Kallaplayam
08048052684
+919943021649

Another factor you may need to consider is the thi...

Another factor you may need to consider is the thickness of the coating of flux on your electrode. This measurement is indicated by a coating factor, which is the ratio of the rod’s diameter and the coating’s diameter. There’s some margin of error, but the three ranges center around these values. Light: A coating factor of around 1.25 Medium: A coating factor of around 1.45 Heavy: A coating factor of 1.6-2.2.
 2025-05-02T05:03:19